What does OSP mean in PCB?
OSP stands for Organic Solderability Preservative — a thin organic film that protects the copper surface until soldering. It is low-cost and flat, but sensitive to handling, heat and humidity, so it suits short storage cycles and controlled assembly.
What is ENIG black pad?
Black pad is excessive nickel corrosion during the immersion gold step, which can cause brittle solder joints. It is controlled through bath chemistry and process management, and assessed by cross-section analysis and joint reliability testing when required — not by visual inspection or XRF.
Is HASL lead-free and RoHS compliant?
Yes — lead-free HASL variants are available, confirmed for our multilayer, high-layer-count and HDI boards. The alloy for an order is confirmed during engineering review. A lead-free finish material alone does not make the whole board RoHS compliant — compliance depends on all materials and applicable exemptions.
How long does ENIG last before assembly?
Common industry and supplier references often specify approximately 12 months for ENIG and HASL, and approximately 6 months for OSP. Actual solderability shelf life depends on the manufacturer's specification, packaging and storage conditions; the guaranteed period for an order is confirmed before production.